Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bcdb7859d196574348806c539e0e92d6 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 |
filingDate |
1999-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c20c4ddb59923a7f7de20e9582c37e74 |
publicationDate |
2000-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2000265011-A |
titleOfInvention |
Flame retardant resin composition |
abstract |
(57) [Summary] [PROBLEMS] To provide good moldability as well as flame-retardant performance, do not generate halogen gas, and provide mechanical properties when formed into a molded product such as an insulating material or a sheath material of electric wires. And a flame-retardant resin composition having excellent heat deterioration properties. SOLUTION: An inorganic flame retardant containing a metal hydrate and antimony oxide is mixed in an amount of 50 to 200 parts by weight and a fine powder of a fluororesin in an amount of 5 to 20 parts by weight based on 100 parts by weight of an olefin resin. A flame-retardant resin composition characterized by the following. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100666257-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2004011548-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004011548-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012059104-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8557906-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015193825-A |
priorityDate |
1999-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |