http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000258868-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 1999-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06b21ff1887629fad94223eaa248b18a |
publicationDate | 2000-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000258868-A |
titleOfInvention | Manufacturing method of photothermographic material |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a photothermographic material having a high Dmax, a small change in photographic sensitivity over time of a coating solution, and a good coated surface. SOLUTION: When forming an image forming layer and a protective layer using a polymer latex binder with a coating solution containing a polymer latex, the liquid film surface temperature during constant rate drying is set to be equal to or higher than the glass transition temperature of the layer, Further, drying is performed by setting the dry bulb temperature at the rate of drying to 80 ° C. or less to produce a photothermographic material. |