abstract |
(57) [Summary] [PROBLEMS] To obtain a cosmetic material excellent in scratch resistance. SOLUTION: An adhesive layer 1, a picture layer 2, a transparent primer layer 3, and a transparent surface protective layer 4 are laminated in this order on a base material B, and the adhesive layer has a glass transition temperature of 62 ° C or lower. Two-part curable urethane resin obtained by crosslinking a polyol with isocyanate, two-part curable urethane resin obtained by crosslinking a transparent primer layer with an acrylic polyol and isocyanate, and a transparent surface protective layer having an acryloyl group or a methacryloyl group in a molecule. It comprises a monomer, a prepolymer, or a polymer obtained by crosslinking at least one of the polymers with ionizing radiation. At least the picture layer is preferably a layer formed by transfer using an elastic roller or solid particle collision pressure for transfer pressure pressing. |