http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000241925-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-015 |
filingDate | 1999-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_109bb86602ca63b0f8ab4399655f5470 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_094d8f3048506d4b119ce14c12964b6f |
publicationDate | 2000-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000241925-A |
titleOfInvention | Method for producing silver halide photographic emulsion and silver halide photographic light-sensitive material using the emulsion |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a silver halide emulsion in which high sensitivity and low fog are maximized by a novel metal doping method, and a silver halide produced by the production method An object of the present invention is to provide a silver halide photographic material using an emulsion. SOLUTION: Metal halide-doped silver halide fine particles are added at a pAg of 8.5 or less during the period from the formation of silver halide grains to after the formation thereof to deposit on the silver halide grains. A method for producing a silver halide photographic emulsion, wherein the pAg at the time of growing silver halide grains is 9.0 or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6793390-B2 |
priorityDate | 1999-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 166.