http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000221648-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C11-00 |
filingDate | 1999-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_52f59398366084f26a37595c59b12662 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2cf0a16884f3d2102b7962333d9fcd0c |
publicationDate | 2000-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000221648-A |
titleOfInvention | Processing method of silver halide photosensitive material |
abstract | (57) [Summary] [Problem] When processing a silver halide photographic light-sensitive material using an automatic developing machine, a washing alternative stabilizing solution or an additive thereof that can prevent generation of scale even if the amount of washing water is reduced. And a method of processing a silver halide photosensitive material using the same. Furthermore, the amount of discharge is reduced by using the overflow solution for washing as dilution water for replenishing the fixing. SOLUTION: In a method for processing a silver halide photographic material in a continuous step having at least a developing step, a fixing step and a washing step, at least one kind of aminopolycarboxylic acid and 5- A treatment method in which the treatment is carried out using an aqueous solution containing sulfosalicylic acid or a salt thereof, and part or all of the overflow is used for replenishing the bath in the fixing step. |
priorityDate | 1999-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.