http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000220631-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5e7f3a21fd28b7f26b172927af2b413 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D99-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 |
filingDate | 1999-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b7aeb33a16309b9e3d5a1e049533cfa |
publicationDate | 2000-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000220631-A |
titleOfInvention | Conductive roller |
abstract | (57) [Summary] [PROBLEMS] In stirring casting into a thermosetting polyurethane resin having excellent wear resistance, a large amount of graphite can be mixed, thereby satisfying the required value of conductivity and maintaining high quality for a long time. Provide a conductive roller. SOLUTION: A conductive roller 20 according to the present invention is formed by casting a roller surface material between a roller shaft outer surface 21 and a mold inner surface 31 surrounding the roller shaft 22 with a predetermined gap 32 therebetween and solidifying the same. The conductive roller 20 is formed so as to cover the roller shaft 22. The roller surface material is obtained by mixing and stirring granular graphite into a thermosetting polyurethane resin 40 and dispersing the mixture so as to obtain conductivity. Was. |
priorityDate | 1999-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297 |
Total number of triples: 15.