http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000191909-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 |
filingDate | 1998-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b59d92fb3f952cc8e0fc72f903749f7d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8b1994c6be0040721389982d2b30be8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c74d4a9d77731faacbca0990f95e9041 |
publicationDate | 2000-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000191909-A |
titleOfInvention | Polyimide resin composition for melt molding with good thermal stability |
abstract | (57) [Summary] [PROBLEMS] To achieve stable melt molding, stable color tone, A product having physical properties can be produced, and the product obtained by molding sufficiently crystallizes without heat treatment, and has high heat resistance, that is, has sufficient mechanical strength even at a temperature equal to or higher than the glass transition temperature. Provided is a polyimide resin composition for melt molding having high heat stability. SOLUTION: The repeating unit 9 represented by the following formula (1) It is composed of 0 to 100 mol% and 10 to 0 mol% of a repeating unit represented by the following formula (2) or (3), has a specified molecular terminal, and is held at 420 ° C. for 5 minutes to be melted. 50 to 95% by weight of a crystalline polyimide having a change in melt viscosity of 50% or less when held at 420 ° C. for 30 minutes, glass fiber, carbon fiber, wholly aromatic polyamide fiber, titanium A polyimide resin composition for melt molding comprising 50 to 5% by weight of one or more fibers selected from potassium acid fibers, silicon carbide fibers, metal fibers, alumina fibers, boron fibers, and graphite fibers. Embedded image |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2798033-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2802448-C1 |
priorityDate | 1998-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links