http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000187339-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B08B3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B08B3-02 |
filingDate | 1998-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7524eff1aea412440744825f9189e6a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ac9344bab15c1c7a8b84974e956ea33 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bcad47de31daf3063e0f806c065dddd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c954d4181fc3e9415e0866dbb503634 |
publicationDate | 2000-07-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000187339-A |
titleOfInvention | Method for cleaning object to be cleaned and method for manufacturing electrophotographic photoreceptor |
abstract | (57) Abstract: Provided is a method for manufacturing an electrophotographic photoreceptor capable of obtaining a uniform and high-quality image without image defects and image density unevenness. SOLUTION: In a method for manufacturing an electrophotographic photosensitive member including a step of forming a functional film on a substrate, particularly on an aluminum substrate containing silicon, iron and copper, an interface is formed before the step of forming the electrophotographic photosensitive member. The substrate surface is degreased and washed with water containing an activator, and the surface of the substrate is washed with water containing at least one of a surfactant, carbon dioxide, and a specific inhibitor. Al, Si and O formed on the surface of the base are mainly used, and the film thickness is 5 After forming a film having a composition within a certain range of not less than {not less than 150}, the surface of the substrate is sprayed with pure water or water in which carbon dioxide is dissolved, or shower water containing an inhibitor to a pressure of 4.9 × 10 3 Pa. or 9.8 × 10 4 Pa and the range, spray flow 1l / min of shower water Shower water is sprayed on the surface of the substrate in the range of not less than 20 l / min. |
priorityDate | 1998-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |