http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000173660-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be055db3c1a09879df07379ba969e223 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 |
filingDate | 1998-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31c67bfccf912a10b63271ce7307e4be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c837c58fa5768c3d0842751d2ea45e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a58ab85eabb5e70998697ed3bca1a8b |
publicationDate | 2000-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000173660-A |
titleOfInvention | Non-aqueous electrolyte secondary battery |
abstract | (57) [Problem] To improve non-electrode material and to improve electrochemical characteristics such as charge-discharge capacity and charge-discharge cycle life by limiting the thickness and piercing strength of a separator located between positive and negative electrodes. A water electrolyte secondary battery is provided. SOLUTION: In a non-aqueous electrolyte secondary battery, as an anode material, composite particles in which the whole or a part of a core particle composed of a solid phase A is coated with a solid phase B, and the solid phase A is silicon, zinc Containing at least one of the following as a constituent element, The solid phase B is any one of the constituent elements of the solid phase A, silicon and zinc, and excluding the constituent elements, a Group 2 element of the periodic table; 1 excluding transition elements, group 12 and 13 elements, and carbon A solid solution with at least one element selected from the group consisting of Group 4 elements or a material that is an intermetallic compound is used, and the thickness of the separator located between the positive and negative electrodes is 15 μm or more and 40 μm or less, and the thickness of the separator is The piercing strength is 200 g or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4674458-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006134757-A |
priorityDate | 1998-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.