http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000160200-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dae64c775f32c43199adbb4389c2c9b3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D17-06 |
filingDate | 1998-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e423199d2a0c877b154de2f3ce33542 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92195f60d49ccbb82aa1de53177559e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0643a1d6f26e49aaed04aa69b1c9a022 |
publicationDate | 2000-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000160200-A |
titleOfInvention | Method for producing compression molded detergent |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a compression molded detergent excellent in disintegration and dispersion characteristics in a short time and with high productivity. SOLUTION: As a step, (1) a detergent composition having the same composition as the pre-granulated granules is stirred and granulated in the presence of the pre-granulated granules to obtain an average particle size of 300. (2) a step of classifying the resulting detergent particles, and (3) a step of compression-molding the resulting detergent particles. I do. |