http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000141473-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D7-01 |
filingDate | 1998-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ce55ce0941cd406b6f49100c4088cca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c9efbe008c98c6114a13f67c7ed899b |
publicationDate | 2000-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000141473-A |
titleOfInvention | Biaxially oriented polyethylene-2,6-naphthalate film |
abstract | (57) [Summary] [PROBLEMS] To obtain a transferred image with small deformation of a film upon heating and excellent in gradation, and further to reduce a bowing phenomenon to obtain a film having uniform physical properties in a width direction. Provided is a film suitable for a thermal transfer ribbon excellent in productivity and excellent in flatness. SOLUTION: This is a biaxially oriented polyester film containing polyethylene-2,6-naphthalate as a main component, and the orientation angle in the width direction of the film is 75 ° or more and 105 ° or more. The Young's modulus in the longitudinal direction (YMD, kg / mm 2 ) and the Young's modulus in the width direction (YTD, kg / mm 2 ) are expressed by the following formula (1). To (3), and the heat shrinkage (SMD,%) in the longitudinal direction and the heat shrinkage (STD,%) in the width direction after heat treatment at 200 ° C. for 10 minutes satisfy the following expression (4). A biaxially oriented polyethylene-2,6-naphthalate film. 700 ≦ YMD (1) 500 ≦ YTD (2) 1.1 ≦ YMD / YTD ≦ 1.4 (3) 0.8 ≦ SMD / STD ≦ 1.3 (4) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005186350-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4604483-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040022264-A |
priorityDate | 1998-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 131.