http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000138134-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be055db3c1a09879df07379ba969e223 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-035 |
filingDate | 1998-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da5c01bf8df79ec46296c0dbb2e19b0d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d16015d014018527cb70e55df703a37b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2352a71df34cd996bd9e2136af27905d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_340e9dee59fcc55a21af882548f6034d |
publicationDate | 2000-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000138134-A |
titleOfInvention | Electrolytic solution for driving aluminum electrolytic capacitor and aluminum electrolytic capacitor using the same |
abstract | (57) [Problem] An anode lead corrosion disconnection occurs even when an aluminum electrolytic capacitor using an electrolytic solution obtained by dissolving an electrolyte in a solvent containing γ-butyrolactone is used for a long time under high temperature and high humidity. It is an object of the present invention to provide a highly reliable aluminum electrolytic capacitor without any problem. SOLUTION: A highly reliable aluminum electrolytic capacitor can be provided by using an electrolytic solution for driving an aluminum electrolytic capacitor comprising a solvent and a solute and having oxycarboxylic acid added in an amount of 0.1 wt% or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006165001-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018198248-A |
priorityDate | 1998-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 113.