http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000129051-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate | 1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed67acba9b52fff946af331734d894f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d35e7924eac119a06580841e4bc2688 |
publicationDate | 2000-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000129051-A |
titleOfInvention | Polypropylene resin composition for film |
abstract | PROBLEM TO BE SOLVED: To reduce the dispersion particles of a rubber component in a resin composition, improve heat seal strength, low temperature heat sealability, and have excellent low temperature impact resistance and transparency. Offer things. The rubber component (B) comprises (A) 50 to 99% by weight of a polypropylene resin and (B) 1 to 50% by weight of a rubber component. 0.875 g / cm 3 , MFR 190 0.1-50 g / 10 an ethylene random copolymer selected from a random copolymer of ethylene and α-olefin having 4 to 20 carbon atoms, (ii) 1-butene content of 60 to 99 mol%, MFR 190 0.1 to A 1-butene-based random copolymer selected from a random copolymer of 50 g / 10 min of 1-butene and an α-olefin having 2 to 20 carbon atoms excluding 1-butene was used at a weight ratio of 95: 5 to 5: 5. : A polypropylene resin composition comprising a random copolymer composition in the range of 95. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000344976-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010053341-A |
priorityDate | 1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 60.