Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_edda5e3167828efc51b03b3964858e45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G19-02 |
filingDate |
1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a1e3793eb359f749e7200a53ffbddbe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ef31b4420b12b347a8e78bae363b25f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b5132ce2bdd16e3e6377a75329a401b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b9ab0c3210cecbfdeddce082b4adf5d |
publicationDate |
2000-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2000128533-A |
titleOfInvention |
Amorphous tin oxide sol and method for producing the same |
abstract |
(57) [Problem] To provide an amorphous tin oxide sol suitable for use as a transparent conductive material having no coloration and good conductivity, and a method for producing the same. The hydrolyzable tin compound is hydrolyzed, An amorphous tin oxide sol obtained by washing in water and then heating in the presence of ammonia to obtain a sol, wherein the amorphous tin oxide sol is obtained by solification in the pH range of 9.5 to 10.5. Is a low quality tin oxide sol. |
priorityDate |
1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |