http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000128514-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294881271413951a95f284b588a68e66 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0562 |
filingDate | 1998-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43980d7a24e40ab9973b913d7316ec10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3dcfa6777d2ec77ddad84b5ad5ea8a7 |
publicationDate | 2000-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000128514-A |
titleOfInvention | Method for producing lithium-containing compound |
abstract | (57) [Problem] To provide a method for producing a lithium-containing compound which can be easily produced at a low temperature. SOLUTION: Using a sol-gel method, Li, Ti and Al To produce a glass-ceramic lithium-containing compound containing P, O and P or O, or a glass-ceramic lithium-containing compound further containing Si. First, a raw material of an organic metal or an inorganic compound is dissolved and mixed in ethanol, nitric acid is added as a catalyst, and then the mixture is heated to 60 ° C. to form a sol and gel. Then, after drying the gel, 300 A first heating is performed at a temperature in the range of 600600 ° C., followed by a second heating at a temperature in the range of 700〜1100 ° C. Since the sol-gel method is used, it can be manufactured at a low temperature. It is preferable to use Li methoxide and titanium butoxide as raw materials. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101575476-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11130700-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6720110-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108511797-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10399886-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7482097-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105680090-A |
priorityDate | 1998-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.