Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-80 |
filingDate |
1998-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c11b3c14124cd980edd8f1c51876903 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1dd55448cf5c0d276a3b6ac675554f80 |
publicationDate |
2000-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2000103909-A |
titleOfInvention |
Method for producing elastomer composition |
abstract |
PROBLEM TO BE SOLVED: To provide a method for producing an olefin elastomer composition having excellent mechanical properties. SOLUTION: The method for producing a partially or completely dynamically crosslinked elastomer composition comprising (A) a crosslinkable elastomer, (B) a thermoplastic resin, and (C) a radical initiator is defined as follows. At the melting temperature T 2 (° C), A method for producing an elastomer composition, comprising first melt-kneading and then melt-kneading at a melting temperature T 3 (° C.). T 1 : 1 minute half-life temperature (° C.) of (C) T 1 -100 <T 2 <T 1 +40 T 2 +1 <T 3 <T 2 +200 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001310963-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015101062-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4758588-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011021146-A |
priorityDate |
1998-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |