http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000095878-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 1998-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44fb43fbb0410eaa035ad239325df0e5 |
publicationDate | 2000-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000095878-A |
titleOfInvention | Method for producing propylene-based resin film |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a propylene-based resin film which is excellent in flexibility, transparency and gloss and has no environmental pollution. SOLUTION: 100 parts by weight of a resin component composed of 97 to 10% by weight of a propylene-based resin and 3 to 90% by weight of a vinyl aromatic elastomer, and 0.005 to 0.1 of a crystal nucleating agent. A method for producing a propylene-based resin film, comprising forming a resin composition consisting of parts by weight at a cooling temperature of 30 to 70 ° C by a T-die method or a downward water-cooled inflation method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100378159-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2287247-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100765008-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8609009-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005059025-A1 |
priorityDate | 1998-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.