http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000086369-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_91dd0486eb68cf8891e94094e783c495 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B38-068 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-20 |
filingDate | 1998-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3dabb7bfd5b82546118dea283a1ba8d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8639e94ea44c1474ff1e98df0835712 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fb306c2e47ca3f056baa71cc8f71aab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f11cc7ec748ee324f718e68ce73c700 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb59cf8aaa3b0e9832a794905b4e8c5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d561c12f11cecc2c7c2cae07cdfa3534 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb3048973b6745d7e8d5fb5a9949c906 |
publicationDate | 2000-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000086369-A |
titleOfInvention | Multifunctional material and manufacturing method thereof |
abstract | (57) [Abstract] [Purpose] Consisting of zeolite ore powder or shale powder and coal powder, excellent water absorption, water permeability, sound absorption, heat insulation, moisture control, deodorant properties under slight molding conditions. In addition to providing functions such as antibacterial properties, inexpensively providing multifunctional materials that retain properties such as water resistance, fire resistance, weather resistance, light weight, etc. And a method for producing the same. [Constitution] Zeolite ore powder or shale powder having a particle size of 1 mm or less is blended with 10 to 60% by weight of coal powder having a particle size of 1 mm or less, In addition, water is added in an appropriate ratio and uniformly dispersed and kneaded with each other to form a raw material. In addition, extrusion molding or press molding is carried out to a required shape and dimensions with a molding pressure of 20 to 300 kg / cm 2. After molding, the residual moisture is 1.0 % By weight, and then heated at a heating gradient of 40 to 80 ° C./hour and fired at 600 to 1050 ° C. to form a porosity of 20 to 90%. A multifunctional material and a method for producing the same. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112961394-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112961394-B |
priorityDate | 1998-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.