http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000086334-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_90dd0fee0bc7677f598b8b631ab210cd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-101 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D41-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C5-46 |
filingDate | 1998-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea7970e4d8543b4e51a8718b4599922b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1556f8bce7cefa0292bc29c26ac10a7f |
publicationDate | 2000-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000086334-A |
titleOfInvention | Brick for sliding nozzle device |
abstract | PROBLEM TO BE SOLVED: To improve the oxidation resistance of an upper nozzle brick for a sliding nozzle, a lower nozzle brick and a plate brick, particularly in an intermediate temperature range of 200 to 700 ° C. It reduces the ragging phenomenon that has occurred, thereby improving the durability of the brick itself. SOLUTION: 0.1 to 10% by weight of carbon black having a specific surface area of 24 m 2 / g or less is added to a blend of a brick for a sliding nozzle comprising a refractory raw material and a metal, and an organic binder is further added. After kneading and molding, A heat treatment is performed at a temperature of 150 to 1000C. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7060642-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106495715-A |
priorityDate | 1998-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.