abstract |
PROBLEM TO BE SOLVED: To provide a laminate excellent in performance such as low-temperature heat sealability, heat seal strength and hot tack property, and improved in workability. SOLUTION: An ethylene / α-olefin copolymer (component A) produced using a metallocene catalyst is 50 to 99% by weight, and has an MFR of 0.1 to 20 g / 10 minutes; MFR containing 1 to 50% by weight of a high-pressure low-density polyethylene (component B) of 93 g / cm 3 , Is 5 to 25 g / 10 min; density is 0.87 to 0.932 g / cm 3 ; ME (3 g) is 1.2 to 2.3; MT is 1.0 A laminate comprising a layer comprising a resin composition having a weight of at least g. |