http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000042523-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33cee5d41e4efa2d29f3331d0c791d6a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_971516b5255324ebb985b5542dd43247 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05C9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B5-00 |
filingDate | 1998-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e00674248da2715d1f87af7b05ef115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92123813aae382d9caae721a506bef93 |
publicationDate | 2000-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000042523-A |
titleOfInvention | Separation method of resin coated steel sheet |
abstract | (57) [Problem] To provide a method for separating a resin-coated steel sheet, which makes it possible to separate the resin part and the steel part of the resin-coated steel sheet easily in a short time and at low cost. SOLUTION: A resin-coated steel plate to be separated is -180. Immerse in a low temperature liquid at a temperature lower than ℃ for a predetermined time. Alternatively, after the resin-coated steel sheet to be separated is immersed in a low-temperature liquid at a temperature lower than -180 ° C for a predetermined time, stress is applied to the resin-coated steel sheet. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009040131-A |
priorityDate | 1998-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 20.