http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000038419-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 1998-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_301687e401d3b58986451ce36dd4c310 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c6af196b49ab72e5d9db86385bd9bfc4 |
publicationDate | 2000-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000038419-A |
titleOfInvention | Ethylene-α-olefin copolymer |
abstract | (57) [Problem] To provide an ethylene-α-olefin copolymer having both sufficient transparency and elasticity when formed into a film without impairing excellent mechanical properties and processability. SOLUTION: A copolymer of ethylene and an α-olefin having 3 to 20 carbon atoms, which satisfies the following conditions (a) to (e). (A) Melt flow rate (MFR): 0.05 to 10 0 g / 10 min (b) Density (d): 0.85 to 0.97 g / cm 3 (c) Melt tension at 190 ° C. (MT (g)) and melt flow rate (MFR (g / 10 min)) Satisfies the following equation: log (MT) ≧ −0.91 × log (MF R) +0.12 (d) Equilibrium compliance (Je) at 190 ° C. is 3. 0 × 10 −4 Pa −1 or more (e) Crystallization start temperature (Tc) is 108 ° C. or more |
priorityDate | 1998-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |