http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000026584-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-688 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 1998-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ae04d8ea62cee7d6f6beab9bac8f801 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e8f26732a8e58463c58ffea4e0d2a57f |
publicationDate | 2000-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000026584-A |
titleOfInvention | Polyester and film comprising it |
abstract | (57) [Summary] [Problem] When producing a polyester film, the adhesiveness on a rotary cooling drum is excellent, the contamination of an electrostatic wire and the attachment of sublimate to an extrusion die are suppressed, and the productivity is excellent and the sanitation is performed. Provided are a polyester resin composition and a polyester film having excellent properties. SOLUTION: The acid component in the polyester is from 0.1 to 0.1%. A polyester comprising 45 mmol% of a sulfonic acid quaternary phosphonium salt having an ester-forming functional group, wherein the amount of diethylene glycol in the polymer is 0.3 to 5.0%. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108624010-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019011453-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002248722-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10351668-B2 |
priorityDate | 1998-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 77.