abstract |
(57) [Summary] [Problem] A high-molecular weight resin for toner can be obtained. Further, the present invention provides a method for producing a resin for a toner, which is excellent in fixability, offset resistance, and blocking resistance. SOLUTION: Styrene and (meth) are prepared by using a polymerization initiator. In the method for producing a resin for a toner which is copolymerized with an acrylate ester, whether at least one selected from the group consisting of dicinnamoyl peroxide and a tertiary alkyl peroxycinnamate having 4 to 8 carbon atoms is used as a polymerization initiator Or a combination thereof with another polymerization initiator having a half-life of 10 hours in benzene and a temperature of 65 to 130 ° C. |