http://rdf.ncbi.nlm.nih.gov/pubchem/patent/IT-1216309-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0769c42f60de3c62542d874953178966 |
filingDate | 1986-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1990-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a7af4ff0968be854f57647f970b0cf3 |
publicationDate | 1990-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | IT-1216309-B |
titleOfInvention | PROCEDURE FOR FORMING POLYMERIZABLE RESIN OBJECTS WITH A FLAT SURFACE, EVEN WITH SUB-TEAMS. |
abstract | Indicator tube detects the presence, with a mimimum concn. of 5x10 power (-3) MG/L, of mixtures of 2,2'-dichlor-tri-ethylamine, methyl-bis-beta-chlor-ethylamine and 2,2',2-tri-chlor-tri-ethylamine. Tube contains a polyethylene insert (2), filler (3) contg. calcium chloride, and superimposed indicator layer (4) of a bismuth salt, pref. bismuth-iodide, and glass wool (5). |