http://rdf.ncbi.nlm.nih.gov/pubchem/patent/HU-0400586-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8510b82803aeb992567f40e50085414b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00482 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-285 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B30-00 |
filingDate | 2004-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ea0c14e1d5dc199c76eb072e303098f |
publicationDate | 2006-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | HU-0400586-A2 |
titleOfInvention | Indoor parget and method of producing thereof |
abstract | The subject of the invention is interior decoration plasterings and.method to produce aesthetic surface with interior decoration plasterings binding easily, to be cleaned easily, removable and of high air-permeability. The interior decoration plasterings according to the invention is of medium strength, to be applied particularly indoors, can be stored for a long time. Characterized by that, it contains 50-90 mass% of powder-like stone rubble classified 00, and 10-50 mass% of stone-powder or stone rubble sieved to suitable size of 1-10 mm, as well as 2-5 mass% of cellulose-base binding materials, preferably tapestry adhesive. The invention furthermore is a method for producing interior decoration plasterings primarily interior decoration plasterings of medium strength, to be applied particularly indoors, which can be stored for a long time. The method is characterized by that, the cellulose-base binding material, preferably tapestry-adhesive is mixed in water till clear-stemmed, then 50-90 mass% of powder-like stone rubble classified 00, and 10-50 mass% of stone-powder or stone rubble is added, mixed butter-like, then the material compiled is mixed again 10-15 minutes after mixing, then it is applied on the prepared wall, then after binding the surface can be used. |