Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d7afd4e02bb9f89612bf84775aaf541a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2219-00121 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2303-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2303-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2219-00189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2103-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2219-00168 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2219-00186 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J13-0008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J19-1881 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-5236 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01F23-00 |
filingDate |
2016-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26c3279062fd48008c883b7681d8a1eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_37e4a910ead062f85f14faf10ea1b50e |
publicationDate |
2017-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
HK-1222384-A1 |
titleOfInvention |
Method and device for preparing hydroxide slurry |
priorityDate |
2013-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |