http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2355984-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a526baeaf0a6e90f4a91d4dbfd619756 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J195-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D195-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-00 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D195-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E01C7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J195-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 |
filingDate | 2000-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10a60cbb0ea78f76ca81a55db72b06da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_324a3c44629a3cddd09a3d2df3bc14f5 |
publicationDate | 2001-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | GB-2355984-A |
titleOfInvention | SBR for asphalt cement modification |
abstract | An SBR used to modify asphalt cement is a blend of (i) a high molecular weight styrene-butadiene rubber having a weight average molecular weight of at least about 300,000 and (ii) a low molecular weight styrene-butadiene rubber having a weight average molecular weight of less than about 280,000; wherein the ratio of the high molecular weight styrene-butadiene rubber to the low molecular weight styrene-butadiene rubber is within the range of about 80:20 to about 25:75; and wherein the bound styrene content of the high molecular weight styrene-butadiene rubber differs from the bound styrene content of the low molecular weight styrene-butadiene rubber by at least 5 percentage points. These SBR compositions are comprised of repeat units which are derived from styrene and 1,3-butadiene, wherein the styrene-butadiene rubber composition has a number average molecular weight as determined by field flow fractionation which is within the range of about 50,000 to 150,000 and wherein the styrene-butadiene rubber has a light scattering to refractive index ratio which is within the range of 1.8 to 3.9. |