Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32681f1832d227fe8df23d12a37f67a8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2363-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-283 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-44 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate |
1987-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69281ee0e847840311d8cd7f759c7268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_94b844db020007724bb22b1909ca961f |
publicationDate |
1989-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
GB-2209339-A |
titleOfInvention |
Method of producing porous polymeric material having open pores |
abstract |
A method of producing a porous polymeric material having open pores comprises the steps of preparing an emulsion slurry by vigorously agitating a mixture comprising a main ingredient, a polyamide hardener, a filler and water, casting said emulsion slurry in a water-impermeable mold, hardening said slurry while it contains the water. The main ingredient is a bisphenol-type epoxy resin added with one or more reactive diluents each having one or more epoxy rings per molecule and added in an amount of 18 to 50wt%, based on 100 wt% of said bisphenol-type epoxy resin. A large size molded product having a high wet bending strength and a complicated contour can be produced. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010138346-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5242635-A |
priorityDate |
1987-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |