http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-1482029-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2170-90 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4238 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 |
filingDate | 1975-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1977-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | GB-1482029-A |
titleOfInvention | Elastomeric resin composition |
abstract | 1482029 Elastomeric composition KAO SOAP CO Ltd 24 Jan 1975 [28 Jan 1974] 3165/75 Heading C3P A non-crystalline elastomeric resin composition consists essentially of a homogeneous blend of 100 parts by weight of I, a homopolymer or a copolymer (85-99À9% by weight) of vinyl chloride, and 110-160 parts by weight of II, a thermoplastic polyester-urethane; this polyester-urethane is formed by reacting an organic urethane-forming diisocyanate with a polyester diol having a M.Wt. of at least 4000 and which has been obtained by reacting a saturated aliphatic C 5 -C 8 dicarboxylic acid with a polyol component consisting essentially of a mixture of (a) 1,6-hexanediol and (b) at least one diol selected from 1,2-propane diol, n-butane 1,3-diol and C 3 - 8 diols with one or more CH 3 -side chains, the molar ratio (a) : (b) being 70 : 30-90 : 10. In the examples vinyl chloride homopolymer is blended with polyester-urethane prepared by the reaction of 4,41- diphenylmethane diisocyanate with poly-1,3- butylene/1,6-hexylene adipate. The diol (b), as well as being n-butane 1,3-diol and 1,6- hexanediol, may also be 1,2-propane diol, neopentyl glycol and trimethylpentane diol. The dicarboxylic acid, as well as being adipic acid, may also be pimelic, suberic or methyl-adipic acids. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0015722-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5547741-A |
priorityDate | 1974-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.