http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-1115897-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1d61075d73ada1c4859ec18bca37179f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2483-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-00 |
filingDate | 1967-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06f6609e48c10e81b6a8a92340381b89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67f1a00e5530c475fdc4c4f02147c774 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4300a148af455b66f6986a71b156d982 |
publicationDate | 1968-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | GB-1115897-A |
titleOfInvention | Polyalkylene oxide-polysiloxane block copolymers and process for preparing same |
abstract | A mixture of block copolymers having the average general formula <FORM:1115897/C3/1> wherein each R is a lower alkyl or phenyl radical, each R1 is a lower alkyl, vinyl or phenyl radical, a has a value from 3 to 10, b has a value from 1 to 14, and Y is derived from a mixture composed of 60 to 95 OH-equivalent per cent of (b1) a polyalkylene-glycol monoether consisting of ethylene-oxide and propylene-oxide units and having a content of 40 to 70% by wt. of oxypropylene units and a mol. wt. of from 1000 to 3000, and 5 to 40 OH-equivalent per cent of (b2) a monohydric alcohol and/or phenol, can be made by reacting together a siloxane of the above formula, except that 10 to 30 mol. per cent of the Y radicals are sulphate radicals and the remainder are Cl atoms, a polyalkyleneglycolmonoether containing 40 to 70% (wt.) of oxypropylene units, the remainder being oxyethylene units and having a mol. wt. of 1000 to 3000, and a monohydric alcohol (e.g. isopropanol or lauryl alcohol) and/or phenol. Examples describe the above preparation of the mixed copolymers. Uses.-For stabilizing polyurethane foams. In Example 1 a stabilized polyurethane foam is made by mixing together a polypropyleneoxide triol, tin octoate, water, triethylenediamine, and the siloxane-polyether stabilizer, and adding thereto trichlorofluoromethane and finally tolylene diisocyanate, and after agitation pouring the mixture into a carton. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-2210934-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4153639-A |
priorityDate | 1966-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.