Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ddc1fe20138e94176c3258f7ddf274f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-643 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C14-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C4-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7734 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C4-12 |
filingDate |
2013-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec8cc9178a186678e2f8526e6e49b548 |
publicationDate |
2014-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
FR-3004709-A1 |
titleOfInvention |
PROCESS FOR PRODUCING OPALESCENT LUMINESCENT INERT MATERIAL |
abstract |
A process for producing a luminescent opalescent inert material comprising the steps of melting glass containing at least 75% silica in a furnace at a temperature of about 1400 ° C, crushing the glass thus produced to form glass frits, for preparing a mixture of sintered and inorganic luminescent dopants, and then melting at a temperature below 1400 ° C, the initial glass preparation step being carried out without the presence of lead. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2651726-C1 |
priorityDate |
2013-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |