http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2985262-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_48a2225671369d65fb78d77302fe1572 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-0481 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-048 |
filingDate | 2011-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b16f451c5f51e3f6b2b1beea731d646c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c3b82c4e63a8914a6c5f8c5652ac1f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f5685deb303dfb6abc018462b60b6ab |
publicationDate | 2013-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-2985262-A1 |
titleOfInvention | METHOD FOR MANUFACTURING POLYESTER BIETIRE FILM |
abstract | The invention relates to a process for manufacturing a polyester film, preferably a polyethylene terephthalate PET film, stretched and comprising crystallites; characterized in that it comprises the following steps: (a) Application of granules, based on polyester (15000 and 50000D), and intrinsic viscosity of between 0.4 and 1.3 dL / g; (b) drying the granules; (c) Possible mixing; (d) extrusion; (e) Cooling; (f) optional coating; (g) Biaxial stretching of the film; (h) optional coating; (i) Thermofixation; (j) Relaxation; (k) film winding; (1) Finishing; (m) Controlling the performance of the polyester film by a method A measuring impact-tensile strength and / or method B sonic module measurement; (n) Taking into account the measurements of step (m) to modify, if necessary, the parameters of at least one of the following steps: (g) and (i), so as to control the resistance to hydrolysis of the film. The invention also relates to a bi-stretched polyester film obtained by the process according to the invention, having a hydrolysis resistance measured in a PCT test 36h 125 ° C MD and given by the retention percentage AR> 70%; tensile impact strength in kJ / m> 300; and / or a global planar sonic module value GPSM in daN / mm> 470. The invention finally relates to a module, a panel or a photovoltaic cell equipped with at least one film according to the invention. |