Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_99505f5f312672820e9f78c254c00a4d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1253 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-9033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8828 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8885 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 |
filingDate |
2011-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e162acab3c5b96da86bc4fa856a8bde9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fdc1fca14cdb0502b676b2b75e959438 |
publicationDate |
2012-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
FR-2972572-A1 |
titleOfInvention |
PROCESS FOR PREPARING AN AIR ELECTRODE, THE ELECTRODE THUS OBTAINED AND USES THEREOF |
abstract |
The present invention relates to a method for preparing a Pr NiO-based air electrode with 0 ≤ x <2, comprising a step of subjecting a ceramic ink comprising NiO Pr and a blowing agent to sintering at a temperature greater than 1000 ° C and less than or equal to 1150 ° C. the present invention also relates to the air electrode thus obtained and its uses. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115084549-A |
priorityDate |
2011-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |