http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2556745-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_76ad374a46566472d3b0e588eaae3f12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-62 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-26 |
filingDate | 1984-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4040f1edd6a2a6ff0f41da00787969e |
publicationDate | 1985-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-2556745-A1 |
titleOfInvention | PROCESS FOR ELECTROLYTICALLY DEPOSITING ALLOYS |
abstract | ACCORDING TO THIS PROCEDURE, TO DEPOSIT ROSE YELLOW GOLD-COPPER-ZINC ALLOYS RESISTANT TO COPPER CHLORIDE TEST FROM AN ELECTROLYTE CONTAINING ZINC IN THE FORM OF A CHELATE, AN ALKALI AND OF ZINC AND THE CATIONS OF AN ALKALI, SODIUM IONS WITH A CONCENTRATION NA SUCH AS 20GL NA THE SOLUBILITY LIMIT, WE WORK WITH A GOLD CONTENT OF AT LEAST 2GL, A GOLD CONTENT OF AT LEAST 2GL, IS USED AS CATIONS OF AN ALKALI. OF COPPER OF AT LEAST 10GL AND A ZINC CONTENT OF AT LEAST 5GL, THE PH VALUES BEING MAINTAINED BETWEEN 9 AND 12, THE TEMPERATURE BETWEEN 50 AND 75C AND THE CONTENT OF CHELATING AGENTS OVER 20GL. APPLICATION IN PARTICULAR TO THE REALIZATION OF HIGHLY CORROSION-RESISTANT ALLOYS. |