http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2537328-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3492a7406879265b1f567f37d98dbbaf |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21F9-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21F9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G56-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21F9-30 |
filingDate | 1983-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc97457f4e73d57c8da5b9b3f66850fc |
publicationDate | 1984-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-2537328-A1 |
titleOfInvention | PROCESS FOR THE REVERSIBLE IMMOBILIZATION OF A SULFATE ASH |
abstract | A.PROCEDE FOR REVERSIBLE IMMOBILIZATION OF SULPHATE ASH. B.PROCESS CHARACTERIZED IN THAT A METAL, SUCH AS ALUMINUM, CERIUM, SAMARIUM OR EUROPIUM, OR A MIXTURE OF THESE METALS, IS ADDED TO THIS ASH; ADD TO THIS ASH A SUFFICIENT QUANTITY OF A MELTING AGENT TO LOWER THE PERCENTAGE OF SULPHATES OF TRANSURANIC ELEMENTS TO A VALUE BETWEEN 1 AND 10, WE HEAT THE RESULTING MIXTURE TO A SUFFICIENT TEMPERATURE TO MELT AND MELT THE METAGENT OR THE ADDITIONAL METALS, COOL DOWN TO A SOLID STATE AND THEN SEPARATE THIS ALLOY FROM THE REST OF THE MIXTURE. C. THE INVENTION APPLIES TO THE RECOVERY OF TRANSURANIAL ELEMENTS FROM SULPHATE ASH. |
priorityDate | 1982-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 35.