http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2507631-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ac595689f28ec52f2187df04f54c4ce |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-60 |
filingDate | 1982-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7299adf1da99640c1b00b5567d61aab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53037a6c9d94a7b41344fa926b983829 |
publicationDate | 1982-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-2507631-A1 |
titleOfInvention | COMPOSITION FOR ELECTROLYTIC TIN DEPOSITION CONTAINING PERFLUOROALKYLSULFONATE AS WETTING AGENT |
abstract | AN ELECTROLYTIC COATING BATH FOR THE HIGH-SPEED DEPOSIT OF SHINY METAL TIN USES TIN FLUOROBORATE AND SULFURIC ACID AS ELECTROLYTE; IN ADDITION TO SOME OTHER ADDITIVES, THE BATH CONTAINS A WETTING AGENT IN THE FORM OF PERFLUOROALKYLSULPHONATE TO PROMOTE ANODIC CORROSION; BRILLIANTS USED IN THE SYSTEM INCLUDE AROMATIC ALKYLS AND AROMATIC ALDEHYDES; FOR SOME PURPOSES, IT MAY BE ADVANTAGEOUS TO INCLUDE BORIC ACID AS PART OF THE ELECTROLYTE, AND IN OTHER CASES, TO USE AROMATIC SULPHONIC ACID TO ENHANCE BATH STABILITY AND SHINE. |
priorityDate | 1981-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 72.