http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2393861-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_79cbb9f87b30f4e71aae70684a99180e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-00 |
filingDate | 1978-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1979-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-2393861-A2 |
titleOfInvention | PROCESS FOR MANUFACTURING YARNS OR FIBERS IN SYNTHETIC MATERIALS |
abstract | The present invention relates to a process for preparing yarns or fibers of plastics, in particular from polymers of high melting point, or non-fusible, or from poorly soluble or insoluble polymers, such as polytetrafluoroethylene, according to which a cylindrical molded mass of synthetic material is rotated in contact with an incision device having a certain number of incision teeth, and in contact with a bay disposed downstream of said incision device, in the direction of rotation, and we remove a ribbon of parallel threads, which we stretch by heating. According to this process, the threads are twisted and drawn in a bath of molten metal, in particular of tin, maintained at a temperature of 300 to 380 degrees C, preferably in two stages, dissolving the residual metal with water. 'acid. The wires thus obtained have a higher resistance. |
priorityDate | 1977-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links