http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2392070-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d816e9611efad49f0f71391032a0bf3f
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G14-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-34
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G14-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-10
filingDate 1978-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 1978-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber FR-2392070-A1
titleOfInvention PROCESS FOR MANUFACTURING A REINFORCED RUBBER
abstract The invention relates to obtaining a reinforced rubber by incorporating a new reinforcing resin. A mixture comprising 100 parts of a rubber, 5 to 150 parts of a carbazole / phenol / formaldehyde resin, 1 to 15 parts of a rubber vulcanizing agent of 5 to 15 parts (per 100 parts) is prepared in the usual way. resin) from a formaldehyde donor. The mixture is then heated, preferably under pressure, to vulcanize the rubber and crosslink the resin. Application: those of conventional reinforced rubbers.
priorityDate 1977-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID712
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425240125
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID996
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6854
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419474448
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425901710

Total number of triples: 21.