http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2616119-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbaf303c809f2f0c0a0d860d329fadbd |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2439-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2439-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-518 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2553-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2013-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_633f1253f8f44a683d4a7b52f82e6ae0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b16bd74f72392356a2cd40ed1429c0d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15dca6192b25e34534492c9f921e2ab1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9610f8a7da7d06da1aeec7702b18ad24 |
publicationDate | 2017-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2616119-T3 |
titleOfInvention | Biaxially stretched polyester sheet containing carbon black as a black pigment, as well as its manufacturing process |
abstract | Biaxially stretched polyester sheet of at least two layers in black with a thickness of 10 to 50 μm, containing less than 2.42% by weight, but more than 1.0% by weight of carbon black, a transparency - measured in accordance with ASTM-D 1033-77 - less than 8%, in no layer contains more than 10% by weight of carbon black and has at least one outer layer A, which contains less than 0.5% by weight of carbon black, presenting the outer layer At a brightness at 60 ° - measured in accordance with DIN 67530 - of at least 70 and this layer having a thickness of at least 0.4 μm at a maximum of 7 μm and the carbon black used has a total PAK content of less than 0.5 ppm and the benzo [a] pyrene content is less than 5 ppb and the carbon black used has a BET - determined surface of in accordance with ASTMD 6556-04 - of> 40 and <500 m² / g and an OAN value of> 40 and less than 200 (measured in accordance with standard A STM D 2414 with DBP (ml / 100g)). |
priorityDate | 2012-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.