assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_05df26656ced0dbca5c34b52cbbb79e4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C2222-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D13-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-56 |
filingDate | 2007-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79493e49c818c4d74cf38b7c3f2a259b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4b9b64f9bc44ed3ab7b7f4082fe6e29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71874e200a94675fb0ac8325483b46f2 |
publicationDate | 2017-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2606921-T3 |
titleOfInvention | Surface pretreatment fluid for the metal to be coated by cationic electrodeposition |
abstract | A metal surface treatment liquid for cationic electrodeposition coating comprising zirconium ions, copper ions and other metal ions, and having a pH of 1.5 to 6.5, wherein: the other metal ions are by at least one selected from the group consisting of tin ions, indium ions, aluminum ions, niobium ions, tantalum ions, yttrium ions, and cerium ions; the concentration of the zirconium ions is in the range of 10 to 10,000 ppm; the concentration ratio of copper ions to zirconium ions is in the range of 0.005 to 1 on a mass basis; the concentration ratio of the other metal ions to copper ions is in the range of 0.1 to 1,000 on a mass basis; and further comprises a hydrolysis condensate of the aminosilane compound, which has been obtained by carrying out the hydrolysis condensation of a silane coupling agent having an amino group. |
priorityDate | 2006-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |