Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-916 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G81-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-00 |
filingDate |
2011-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fac57c0fadb0117cd7cef01ee792ea70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad81c96a6682be3d8aaa6094b2a331cc |
publicationDate |
2014-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
ES-2524578-T3 |
titleOfInvention |
Procedure to increase the molecular weight of polyesters |
abstract |
Procedure to increase the molecular weight of polyesters, by heating 100 parts of polyester with i) from 0.01 to 5 parts of a tetracarboxylic acid dianhydride and ii) from 0.01 to 5 parts of a copolymer containing epoxide groups a styrene base, acrylic acid ester and / or methacrylic acid ester in the extruder up to 160 to 350 ° C. |