http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2427444-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_051d5c2f0f0541cfcfa88d350683f235 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-783 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-78 |
filingDate | 2012-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19790d0214eea062c8d64d6de20ea146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ed2f51f8f7981f1fad3165a1bccbd76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17b16f70e88724b424947d3b3bac2571 |
publicationDate | 2013-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2427444-T3 |
titleOfInvention | Procedure for forming gas detection layers |
abstract | Process for forming a porous colorimetric gas detection layer, comprising the following subsequent steps: a) providing a mixture (3) of: an organic solvent, a polymer-forming material, and a gas or particle detection gas detection compound. gas; b) depositing the mixture (3) on at least a portion of the surface (7) of a substrate (5); characterized in that c) an atmospheric pressure plasma (9) is applied to the surface portion (7) to form a polymer layer (11) comprising the gas detection compound or particles; and preferably d) steps b) and c) are repeated several times to form a plurality of stacked polymer layers (11) comprising the gas detection compound or particles. |