abstract |
Aqueous dispersion of polymer P containing 0.1 to 10% by weight of additives of the general formula I ** Formula ** with R1, R2, R3, R4, R5, R6> = H, alkyl with 1 an atoms of carbon, R1 to R6 being both the same as well as different, X, Y> = Cl, Br, I, and n, m> = 1-8, the aqueous dispersion of polymers being obtainable by aqueous emulsion polymerization through radicals of a mixture of monomers containing a) 45 to 70 parts by weight of at least one monomer, whose homopolymer has a glass transition temperature Tg <20 ° C, b) 30 to 55 parts by weight of at least one monomer, whose homopolymer it has a glass transition temperature Tg> 50 ° C, as well as c) 0 to 30 parts by weight of other monomers. |