http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2380573-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_16282a8219b513b82234220e9ab68636 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1352 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2067-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B2009-168 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B2009-165 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B9-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-90 |
filingDate | 2006-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f12d09ad7571ab3fac7f7d4977197db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_578079203931784132ffa8a22f2760d2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e51707d571701e515f5132b08182a52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d0042744a577927875f623353f5f0cd |
publicationDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2380573-T3 |
titleOfInvention | Procedure and device for reducing the content of polyester granulate acetaldehyde |
abstract | Procedure for the preparation of a granulate with low acetaldehyde content from a highly viscous polyester melt with a V.I. between 0.60 and 1.0 dl / g, characterized in that a) the molten polyester bar is fractionated under water at a temperature of at least 90 ° C, b) the accompanying water is separated from the granulate with the least possible cooling of the granulate , so that the granulate present after the separation of the water at a temperature of at least 130 ° C, c) the water-poor granulate thus obtained after the separation of the water is added to a desaldehydration vessel, and d) the granulate in the Desaldehydration vessel is treated by a stream of washing air with an inlet temperature between 180 ° C and 200 ° C, the residence time of the granulate in the desaldehydration part of the vessel increasing to 3 to 20 hours; and the granulate being added in step c) either directly to the desaldehydration vessel or by adding a dosage unit, preferably a cell wheel lock, to the desaldehydration vessel. |
priorityDate | 2005-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |