http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2372951-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_58360af4d88e437dd47d7fb42c4efd00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B31-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-384 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-384 |
filingDate | 2011-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3df0301c0de318de2cb888be7c2a40a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc6fc459ea6e0618b7c5ae34e9751981 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c445015b3903d5be01da51ab2035f8c0 |
publicationDate | 2012-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2372951-A1 |
titleOfInvention | METHOD OF AGLOMERATION OF CARBON MATERIALS. |
abstract | Agglomeration method of carbonaceous materialsnwhich comprises the stages of:n n n n n -n n n Mix the carbonaceous material with oilnsunflower as a binder, until the formation of a pastenhomogeneous,n n n n n n n -n n n Shakenmixing and adding small amounts of carbonaceous material innpowder while stirring the mixture,n n n n n n n -n n n Sift the granular materialnobtained,n n n n n n n -n n n Tryngranular material sifted in air at temperatures aboven220ºC and below 270ºC,n n n n n n n -n n n Cool heated granular materialnYn n n n n n n -n n n Raisenthe temperature of the granular material at temperatures aboven400 ° C in selected atmosphere between inert or poor innoxygen. |
priorityDate | 2011-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.