http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2355770-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b8be6a6c990669567cc455d32b00535e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 |
filingDate | 2007-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad0af757b32198f779ad908bbfc6a152 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8fee23eb7c1be71fc71425819879aa4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d1c01b24d389bae4d044e75ee91b313 |
publicationDate | 2011-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2355770-T3 |
titleOfInvention | PROCEDURE FOR THE PREPARATION OF A RETICULATED RUBBER ARTICLE. |
abstract | The process for preparing a crosslinked rubber article comprising the steps of: a) applying a sulfur containing composition to the surface of a crosslinkable rubber article containing preformed peroxide to provide a sulfur coated article, and b) crosslinking the rubber by heating the sulfur coated article, optionally in the presence of air, at a temperature in the range of 80 to 300 ° C to obtain the crosslinked rubber article. |