http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2241062-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_10852a12bf71364ae81ea61e4066fcd5 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-80 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate | 1997-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64e63998ef54ca8e8134795e681f3a53 |
publicationDate | 2005-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2241062-T3 |
titleOfInvention | IMPROVED MATERIAL OF IMPROVED POLIVINILSILOXANO. |
abstract | THE PRESENT INVENTION REFERS TO IMPROVED COMPOSITIONS OF POLYMERIZABLE POLYGANOSILOXANE WITH TWO COMPONENTS THAT ARE INTENDED FOR USE SPECIALLY IN THE MANUFACTURE OF DENTAL IMPRESSES AND THAT HAVE A BETTER WATERPROOF AND WEAR RESISTANCE. THE IMPROVEMENT OF WEAR RESISTANCE MUST BE IMPROVED TO THE INCLUSION OF A QUADRIFUNCTIONAL POLYSYLOXAN WITH A VINYL CONTENT INCLUDED BETWEEN 0.16 AND 0.24 M - MOLES / G. WORK TIME IS MAINTAINED BY ENTERING SUFFICIENT AMOUNTS OF A RETARDING COMPOSITION THAT DELAYS THE PRINCIPLE OF VINYL POLYMERIZATION. IMPROVEMENT OF IMPROVEMENT BY INTRODUCING A TENSIOACTIVE ACTIVITY THAT IMPLIES THE FORMATION OF AN ANGLE OF SURFACE CONTACT WITH WATER THREE MINUTES BELOW 50 DEGREES. THE SELECTED TENSIOACTIVE HAS A LIPOFILA HYDROPHYL RELATIONSHIP UNDERSTANDED BETWEEN 8 AND 11 SO THAT THE CONTACT ANGLE IS FORMED IN LESS THAN TWO MINUTES AND IS WET IN THE WORK TIME OF THE FOOTPRINT, WHICH IMPROVES THE CUTTING SOFTEN. . THE LOW VISCOSITY FOOTPRINT MATERIAL THAT IS USED INCLUDES A BASE COMPONENT AND A CATALYTIC COMPONENT. BOTH COMPONENTS ARE OF SILOXANE-BASED MATERIALS. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018178451-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2685266-A1 |
priorityDate | 1996-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.