http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2121206-T3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1c1a181abc5ca6f54820b4e9bbc55bce |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-9238 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-92247 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-92209 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-926 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-05 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-92 |
filingDate | 1994-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1998-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f883e5aa35ad8bc3a18b1c3f2d96ed1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c43224658f3960441aa2c4518fc1617 |
publicationDate | 1998-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | ES-2121206-T3 |
titleOfInvention | CONTROL OF THE CONCENTRATION OF A SPINNING SOLUTION INTENDED FOR THE PREPARATION OF A PRODUCT. |
abstract | CONTROL ELEMENTS ARE PRESENTED TO CONTROL THE CONCENTRATION OF IMPURITIES OF A CELLULOSE / AMOX OXIDE / WATER SOLUTION TO BE USED IN THE MANUFACTURE OF CONTINUOUS CELLULOSE FILAMENTS SPREADED WITH SOLVENTS. IMPURITIES CAN BE FORMED BY PREPARING A MIXTURE OF CELLULOSE AMINE OXIDE SOLVENT AND WATER AND HEATING THE MIXTURE TO REMOVE THE EXCESSIVE WATER TO FORM A SOLUTION OF IMPURITIES TO A CONTINUOUS MATCH. FIBERS FROM THE IMPURITIES BELOW TREATED TO FORM THE CELLULOSE FILAMENTS SPIN WITH SOLVENTS. THE CONCENTRATION OF THE SOLUTION IS CONTROLLED BY MEASURING ITS INDEX OF REFRACTION AND MAINTAINING THE INDEX OF REFRACTION WITHIN SPECIFIC LIMITS BASED ON ADJUSTING THE CONTENT OF WATER IN ORDER TO ENSURE THAT THE CONCENTRATION OF IMPURITIES IS SUCH AS IS OBTAINED. |
priorityDate | 1993-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |