abstract |
A resin composition comprising: an ethylene-vinyl acetate copolymer (A); and a propylene-based resin (B), wherein the melt flow rate (MFR: 190°C, 2.16 kg) MFR (A) of the ethylene-vinyl acetate copolymer (A) and the melt flow rate (MFR: 190°C, 2.16 kg) MFR (B) of the propylene-based resin (B) satisfy relational expression (i) below, and wherein the resin composition has an endothermic peak at 120 to 170°C in DSC (differential scanning calorimeter) measurement and has a heat of fusion of 15 to 40 mJ/mg at 120 to 170°C: 4 g/10 min ≤ MFR (A) - MFR (B) ≤ 35 g/10 min. (i) |